Korozijska otpornost legure SS 18/8, legure SS316L, zlata 18 karata i zlata 22 karata u veštačkoj pljuvački u odsustvu i prisustvu tableta eritromicina 500mg

Autori

  • Vincent Agnes Brigitta SBM college of engineering and Technology, Department of Chemistry, Thamaraipadi, Dindigul, Tamil Nadu, India Autor
  • Chinnaiyan Thangavelu EVR Govt Arts College, Trichy, India Autor
  • Susai Rajendran St. Antony's College of Arts and Science For Women, Research Center, Department of Chemistry, Thamaraipadi, Dindigul,Tamil Nadu, India Autor
  • Hashem Abdulhameed Al Kuwait Institute for Scientific Research (KISR), Petroleum Research Center, Kuwait Autor

DOI:

https://doi.org/10.5937/ZasMat1802182V

Ključne reči:

otpornost na koroziju, ispitivanje polarizacije, ortodontska žica, legure SS18/8, legure SS316L, zlato 18 karata, zlato 22 karata, eritromicin

Apstrakt

Otpornost na koroziju legure SS 18/8, legure SS316L, zlata 18 karata i zlata 22 karata u veštačkoj pljuvački u odsustvu i prisustvu tablete Erithromicin 500 mg je procenjena elektrohemijskim ispitivanjem, kao što je ispitivanje polarizacije. Za leguru SS316L, zlato 18 karata i zlato 22 karata, studija polarizacije dovodi do zaključka da se otpornost na koroziju legure SS316L, Gold 18 karata i Gold 22 karata smanjuje u redosledu: AS + Erithromicin> AS. Stoga, ljudi koji u sebi imaju ortodontsku žicu izrađenu od legure SS316, zlato 18 karata i zlato 22 karata, mogu uzimati Eritromicin tablete oralno bez ikakvih oklevanja. Za leguru SS 18/8, studija polarizacije dovodi do zaključka da se otpornost na koroziju legure SS 18/8 smanjuje u redosledu: AS> AS + Erithromicin. Dakle, ljudi koji u imaju u sebi ortodontsku žicu izrađenu od legure SS 18/8, treba izbegavati uzimanje Eritromicin tablete oralno.