Mehanohemijsko-termički postupak dobijanja maskirnog pigmenta

Autori

  • Milan Petrov Institute of Technology of Nuclear and Other Mineral Row Materials - ITNMS, Belgrade, Serbia Autor
  • Miroslav Sokić Institute of Technology of Nuclear and Other Mineral Row Materials - ITNMS, Belgrade, Serbia Autor
  • Zvonko Gulišija Institute of Technology of Nuclear and Other Mineral Row Materials - ITNMS, Belgrade, Serbia Autor
  • Vladislav Matković Institute of Technology of Nuclear and Other Mineral Row Materials - ITNMS, Belgrade, Serbia Autor
  • Ljubiša Andrić Institute of Technology of Nuclear and Other Mineral Row Materials - ITNMS, Belgrade, Serbia Autor
  • Jovica Stojanović Institute of Technology of Nuclear and Other Mineral Row Materials - ITNMS, Belgrade, Serbia Autor

DOI:

https://doi.org/10.5937/ZasMat1404413P

Ključne reči:

spinel, mehanohemijska aktivacija, vibracioni mehanoaktivator, žarenje

Apstrakt

U ovom radu je ispitivana mogućnost dobijanja maskirnog pigmenta mehanohemijsko termičkim postupkom kao i energetsko učešće mehanohemijskog tretmana u dobijanju maskirnog pigmenta stehiometrijske formule Co0,51Zn0,29Mg0,41Cr1,24Al0,24Ti0,31O4. Mehanohemijski i termički tretirani uzorci smeše oksida radi dobijanja kompleksnog spinela su eksperimentalno istraživani u više serija opita, pri čemu su menjani parametri vezani za rad visokoenergetskog vibracionog mehanoaktivatora. Mehanohemijskom aktivacijom smeše oksida (Cr2O3, CO-oksida, ZnO, TiO2, MgO i Al2O3), u vibracionom mehanoaktivatoru sa prstenovima od 30; 60 i 90 min, a zatim termičkim tretiranjem u elektrootpornoj peći, pri vremenu zadržavanja uzorka od 1h, dobija se materijal spinelne strukture koji je pogodan kao maskirni pigment u vojnoj industriji.